OK my first reloads went bang just like they were supposed to but I had some leading with my cast bullets. I had cast ww straight and air cooled them. I was told that was too soft so tonight I made up a new batch. I added some wiping solder to my ww mix, it is supposedly a 63/37 mix, in a 6 to 1 ratio. I also quenched the fresh bullets by dropping them gently into ice water out of the mold. I also made a batch and am letting them air dry only to see if that works also. My first batches of straight ww weighed in at 128gn in my 125gn mold. These new ones weighed in at 124gn so i know I got some tin into them at least. They should be ready to load in a couple of days.